TECHNET Archives

November 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Guy Ramsey <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 12 Nov 2013 18:08:17 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<045e01cedfd0$9dbfd6f0$d93f84d0$@com>
MIME-Version:
1.0
Content-Type:
text/plain; charset="iso-8859-1"
Parts/Attachments:
text/plain (188 lines)
Ha, that possibly is why I can't remember exactly what is the impact ;-).  Thanks.  (not going to buy Ginkgo Biloba at least for now).  

Joyce Koo
Researcher
Materials Interconnect Lab
Office: (519) 888-7465 79945
BlackBerry: (226) 220-4760


-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]] 
Sent: Tuesday, November 12, 2013 12:57 PM
To: 'TechNet E-Mail Forum'; Joyce Koo
Subject: RE: [TN] SnBi solder and SAC solder balls

Oh I been Googling! 

The long and short of it is, no-one can know without understanding the whole
solder system.

My gut tells me the result wouldn't be unreliable in an environment with
thermal excursions below 100C, and service life less than 5 years, but
Murphy was an optimist.

The solder charge combination of SAC38 from Samtec's part and the mix of
SnBi solder paste, with process variation during reflow, make a very complex
and difficult system to optimize and model.  Better to stay SnPb and order
the part with SnPb solder charge.

Some of the aging properties of SAC305 are a little frightening for long
service products.   

Guy

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Monday, November 11, 2013 6:15 PM
To: [log in to unmask]
Subject: Re: [TN] SnBi solder and SAC solder balls

I remember something about internal oxidation SAC plus Bi.   Can't remember
exactly what impact on reliability.   You might want to goggle it.

  Original Message
From: Mike Fenner
Sent: Monday, November 11, 2013 5:26 PM
To: [log in to unmask]
Reply To: [log in to unmask]
Subject: Re: [TN] SnBi solder and SAC solder balls


Guy
To address your last question first: No I don't believe that mixing Sn/Ag/Cu
with Bi/Sn will produce the possibility of a reduced melting temperature
intermetallic zone forming in your solder joints analogous to those reported
when mixing Sn/Pb with SAC. (Sn/Pb/Bi MP around 100C). The lowest melting
range combination pair of constituents is already present (Sn/Bi at 138C).

For your other queries: Welcome to Conjecture World!
We can note
1) That the properties of Sn/Bi have been found to be improved by the
addition of silver.
2) That "reinforced SAC" or "enhanced SAC" alloys have been developed by the
addition of small alloying additions of Bismuth and other stuff.
Patented alloys which have enhanced thermal cycling abilities, temp
withstand etc from these additions are available from certain suppliers, and
are reasonably well documented and have been in use in high rel apps (auto
etc) for some years.

So that sounds kind of favourable. what will actually happen will depend on
the actual alloy mix you form, how homogenous it is, the stresses that the
assembly will see in service and the service life you are looking for. You
might be able to puzzle something out from phase diagrams but you have a lot
of variables, I can understand binary diagrams,(2D) and cope with ternary
(3D) but  I can't do 4D or more. Not many people can - do four dimensions
that is. You need a proper metallurgist or to talk to someone who has gone
before you. In that respect I did get the link in the NASA report given by
Dave to work by a little jiggery pokery (it doesn't seem to work direct). I
did a quick scan through. It's longer than I can cope with at this time of
night, but it looks as though it might be helpful.
It's below


https://tdglobal.ksc.nasa.gov/servlet/sm.web.Fetch/TEERM_LFE_JTR_FINAL.pdf?r
hid=1000&did=41742&type=released

Sorry not to be more specific, maybe others with more direct experience can
be more helpful.

Regards

Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Monday, November 11, 2013 1:30 PM
To: [log in to unmask]
Subject: Re: [TN] SnBi solder and SAC solder balls

Hi Guy - The NASA DoD Lead-free Project did test SAC solders with SnBi
surface finishes so that information may be helpful (not exactly what you
are looking for). The project results can be found on at:

http://www.teerm.nasa.gov/NASA_DODLeadFreeElectronics_Proj2.htm


Honeywell and Celestica have also published an investigation on tin/bismuth
solders - check the APEX proceedings for that information.


Dave Hillman
Rockwell Collins
[log in to unmask]



From:   Guy Ramsey <[log in to unmask]>
To:     <[log in to unmask]>
Date:   11/11/2013 07:19 AM
Subject:        [TN] SnBi solder and SAC solder balls
Sent by:        TechNet <[log in to unmask]>



We have a customer in Korea using Samtec ?Solder Charge? connectors.  The
alloy is SAC38 ( 95.5, 3.8, 0.7).

They want to stay Pb-free.



Our 60 layer, 480mm by  585 mm by  6.5 mm thick board, with  6100+ embedded
capacitors cannot survive the Z axis expansion seen at SAC reflow.  Test
samples have survived 10 reflows at 210°C.



Has anyone tried to qualify the performance of SAC solder with SnBi solder
paste?  Does it have the same problems associated with mixing SAC and SnPb
paste?



Thanks,

Guy


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2