Parts/Attachments: |
|
|
Must be some way. I see materials on it that were added in the last 5
years. If the spec is inactive, the QPL should be as well. Funny how
materials come and go on it.
Lloyd Duso
General Manager
Diamond-MT
(814) 535-3505
www.Diamond-mt.com
On Fri, Sep 27, 2019 at 11:01 AM Douglas Pauls <
[log in to unmask]> wrote:
> Short answer - You Can't. The QPL goes with MIL-I-46058 and that has been
> inactive since 1995. They are "thinking" of revising it, but nothing to
> date.
> IPC-CC-830 has a procedure for adding new classes of coatings, which is
> found in IPC-CC-830 Rev C, Appendix D (I think).
>
> *Douglas Pauls *| Principal Materials and Process Engr | Advanced
> Operations Engineering
>
> *COLLINS AEROSPACE*
>
> 400 Collins Road NE, MS 108-101, Cedar Rapids, IA 52498 USA
>
> *Tel:* +1 319 295 2109 | *Mobile: *+1 319 431 3773
>
> [log in to unmask]
>
> [log in to unmask] for all Export Compliant Items
>
>
> On Fri, Sep 27, 2019 at 9:53 AM Richard Kraszewski <
> [log in to unmask]> wrote:
>
> > What is the process to get a new coating added to the QPL?
> > I haven't done this in a few (ok more than a few) years.
> > Is this still even possible?
> >
> > Rich Kraszewski
> > Senior Staff Process Engineer
> >
> > * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
> >
> > This e-mail and any attachments are confidential from Plexus Corp. and
> may
> > contain information which is privileged, confidential, and/or protected
> by
> > non-disclosure agreements. They are intended solely for the use of the
> > named addressee(s). . Any unauthorized use or disclosure may be
> > unlawful. If you are not a named addressee, you must not use, disclose,
> > retain or reproduce all or any part of the information contained in this
> > e-mail or any attachments If you have received this transmission in
> error,
> > please destroy it and notify us immediately by return e-mail or by
> calling
> > + 1 888 208 9005.
> >
>
|
|
|