The issue is delicate - much more things to consider.

The ultimate source on contact physics is
Holm, R.: Electric Contacts - Theory and Application, 1967

an alternative (and easier available) is
Slade, P.: Electrical Contacts -Principles and Applications, Decker Inc.,
1999

Thomas

> -----Original Message-----
> From: - Bogert [mailto:[log in to unmask]]
> Sent: Friday, February 11, 2005 12:39 AM
> Subject: Calculate current capacity for electrical contacts
>
>
> February 10, 2005
>
> How does one determine what current can be carried by
> electrical connector contacts to determine capability to
> carry about 80 AMPs (RMS), low freq AC, or DC.
>
> We have an application that uses a carbon steel base metal
> pin contact.  The contact is given a nickel flash, followed
> by a copper plating (to fill in small voids), followed by
> another nickel flash, followed by silver plating.  Does one
> calculate current capacity from just the carbon steel base
> metal, or does one need to take the plating into account?
> What formula or chart is used to support the calculation?  If
> the nickel flash thickness is increased, will it impact
> current capacity?  If plating is changed to gold, does that
> impact current
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send
> e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail
> to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> capacity?
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2