Hello everyone,
I used white tin finish on our medium-sized board which has several high
count BGAs. The boards looked nice and the finish was very flat. However,
our assembler reported problems soldering to it, like voids in BGAs and
similar issues (no shorts or opens though). They also recommended HASL as a
preferred finish. This does not sound right to me since HASL will not be as
flat as white tin.
I am thinking that they may have used wrong solder paste and/or did not use
enough of it. If I am on a right track, what solder paste is preferred for
white tin? Are there more gotchas for the white tin process? Would other
finishes like HASL or OSP be better for the board?
Thanks,
Mike Khusid
> -----Original Message-----
> From: DJ Robison [mailto:[log in to unmask]]
> Sent: Tuesday, February 06, 2001 3:08 PM
> To: [log in to unmask]
> Subject: Re: [TN] White tin
>
>
> I've used Omikrom quite a bit. I prefer it to bright acid. It
> has better
> coverage and is an easier process. The only negative so far
> is that it may
> react to some Flux's by staining.
>
> DJ Robison
> Process Engineering Technician
> TTM Technologies, Inc.
> Redmond Division
> 17550 NE 67th Court
> Redmond, WA. 98052
> (425) 883-7575 ext. 229
> [log in to unmask]
>
>
>
> -----Original Message-----
> From: crbuerke [SMTP:[log in to unmask]]
> Sent: Tuesday, February 06, 2001 11:43 AM
> To: [log in to unmask]
> Subject: [TN] White tin
>
> Would like to hear about any experiences anyone has
> with respect to the Omikron white tin immersion
> process used on boards.
>
> Chuck Buerke
> Photonics Systems
> Toledo, Ohio
>
> __________________________________________________
> Do You Yahoo!?
> Yahoo! Auctions - Buy the things you want at great prices.
> http://auctions.yahoo.com/
>
> --------------------------------------------------------------
> ----------
> ---------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following
> message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources
> & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700
> ext.5315
> --------------------------------------------------------------
> ----------
> ---------
>
> --------------------------------------------------------------
> -------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following
> message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources
> & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm)
> for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> --------------------------------------------------------------
> -------------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|