I apologize if I have this wrong: Matsushita Communication Industrial Co
the parent company of Panasonic, is still that; however Matsushita
Electric
Industrial Co., Ltd. is no longer; this was the division that produced the
laminates.
They still do; but with the closing of the factory in North America and
the
gobbling up of the division by the parent, it has become much harder to
get
information. Focus on the central statement: it is hard to get information
on
Japanese and Chinese laminates.
Phil Nutting <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/19/2006 10:15 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Phil Nutting <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Rohs Weeeeeee board material
Added info on Panasonic v. Matsushita
http://foxweb.marist.edu/users/prema.nakra/matsushita.html
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Friday, May 19, 2006 10:10 AM
To: [log in to unmask]
Subject: Re: [TN] Rohs Weeeeeee board material
I thought Panasonic has long been a consumer electronics division of
Matsushita? Guess I was asleep for that memo.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Valerie St. Cyr
Sent: Friday, May 19, 2006 9:56 AM
To: [log in to unmask]
Subject: Re: [TN] Rohs Weeeeeee board material
I am not associated with any laminate company and am not endorsing
anything, but
I don't agree.
Isola just completed the acquisition a month ago. If you look at their
site they have
completed all the transfers with UL and that file is up ..
and they have imported all the slash sheet values, basically just
porting
over
the Polyclad sheets and changing the name and graphics in the header.
http://www.isola-group.com/en/products/name/detail.shtml?47
http://www.isola-group.com/en/products/CompatibleLaminate.pdf
I am much more frustrated with trying to get information on the Japanese
or Chinese
laminates; check Panasonic who bought Matsushita .... and try to find
property values. We have a supplier who wants us to use a laminate that
I can't find on the internet at all! now that bothers me
Valerie
Werner Engelmaier <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/18/2006 08:02 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
Re: [TN] Rohs Weeeeeee board material
Hi Eddie,
Yes, indeed Isola continues to offer the 370HR and other Polyclad
materials,
but it is now more difficult to get the propertiies if yoou look at the
Isola
website. Fortunately, last time I looked, the Polyclad website was still
operating.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|