Easy peazy: 80 Deg C, 10 bars 1-2 hs. depending on a lot. You may
experiment a little. Metallurgists are right, I understand well, because
I've done thousands of plugs myself. Do you use carusel , single or hand
polishing? Finest stage: use diamond slurry? What size ?
Inge
On 4 January 2013 17:23, Ramakrishnan Saravanan <[log in to unmask]>wrote:
> We are making space quality MLBs. We are using hot mounting for micro
> section.
> My understanding is hot mounting(Phenolic power of Buehler at 150 Deg C
> ,180 bar & 5 minutes) of PCB specimen will destroy the PCB specimen Our
> metallographers are against using cold mounting. The reason is they claim
> poor edge retention & high shrinkage and observing faults are difficult.
>
> Which method of mounting is best for micro sectioning PCB ?. Which is the
> best resin & hardener having low shrinkage and high edge retention ?.
>
> regards,
>
> R.Saravanan
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|