TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
Old-Return-Path:
Date:
Thu, 24 Apr 97 07:48:04 -0500
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
Content-Transfer-Encoding:
7bit
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12207
TO:
Return-Path:
<TechNet-request>
From [log in to unmask] Tue Apr 29 09:
38:34 1997
X-Status:
Resent-Message-ID:
<"odtLI1.0.D8A.-ErNp"@ipc>
Subject:
From:
"Ron Hollandsworth"<[log in to unmask]>
X-Loop:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wKNl1-000BjAC; Thu, 24 Apr 97 07:36 CDT
X-Mailer:
ccMail Link to SMTP R6.00.01
Message-Id:
Parts/Attachments:
text/plain (28 lines)

     Elizabeth:
     What is your conveyor speed and conveyor angle?  What type of machine 
     do you have?  Surface tension/peel off upon exit from the wave is 
     usually critical.  Is your flux and mask compatible?  What is the 
     purity level of your solder?  Have you tried changing the board 
     orientation as it goes through the wave?
     
     With no-clean flux conveyor speeds could reach six feet per minute.  
     Normal conveyor angle is usually around seven degrees.  The above 
     questions are some things you may want to check as far as your setups 
     and process.  
     
     [log in to unmask]


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2