Ken,
You didn't say if the board is a multilayer, if so, you may need to
check lay-up construction for metal distribution. Uneven stackup can be
a major cause of warp. We are a pcb vendor and we do not regularly
'dewarp' boards.
Anne Ledger
EMDS, Inc.
> -----Original Message-----
> From: Ken Nevius [SMTP:[log in to unmask]]
> Sent: Tuesday, January 19, 1999 4:33 PM
> To: [log in to unmask]
> Subject: [TN] Bowed Boards
>
> We have been seeing boards come off our reflow oven with bow and
> twist
> that exceeds IPC specs. Our vendor insists that we are the only
> customer that complains about this. We had our reflow oven
> calibrated
> and it looked fine. The only thing about the profile that may be
> suspect is the cooling rate may be a little too fast. According
> to the
> vendor, they put all of their boards through a de-warping process.
> The vendor has tweaked their de-warping process to cool slower in
> an
> effort to make the problem go away.
>
> My question is: This is our first bout with warping, what should
> we be
> looking at for a cause? Is it normal for a pc board vendor to
> have to
> de-warp boards?
>
>
> Regards,
>
> Ken Nevius
> Veeder-Root
> Altoona, Pennsylvania
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|