Peter,
You mentioned that you experience intermittent BGA failures. How were
these failures confirmed and were they isolated to a specific BGA. If so,
a cross section would reveal several artifacts as to the nature of the
intermittent condition. I too have witness suspect nonwet conditions which
was also confirmed by a BGA peel/shear test. Finally sem/edx work
condicuted. Several CAUSES for intermitten can be found. Any real
destructive photos you can share with me on/off line. Be happy to share
with you my two cents worth.
victor,
-----Original Message-----
From: Rick Thompson [mailto:[log in to unmask]]
Sent: Wednesday, September 18, 2002 9:23 AM
To: [log in to unmask]
Subject: Re: [TN] BGA failure and Rework
Peter,
There was a discussion of this in regards to a particular vendor on Technet
about 2 years ago. You can probably find something in the Technet archives
on it.
Rick Thompson
Sr. SMT Process Engineer
SMTEK International, Inc.
+1 (805) 532-2800
[log in to unmask]
===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
9/17/02 5:23 pm
>Technet,
>
>If I may continue my question on BGA rework process:
>
>Recently we have seen intermitted failures from a few BGA assemblies.
>After removing the suspicious BGA on the rework station we noticed
>dewetting on a majority number of pads of the removed BGA. The solder
>ball residues were mostly attaching to the board.
>
>Has anyone seen this before? How likely can this be caused by a
>non-optimum rework removal profile Is baking of the board normal prior
>to rework (removal/re-placement)?
>
>We are tackling this issue from the part supplier side and looking at
>performing destructive X-ray analysis. Can someone give me an idea of
>what the ball attachment process is on the BGA?
>
>Rgds,
>Peter
>
>---------------------------------------------------------------------------
>------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>---------------------------------------------------------------------------
>------
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|