Karl
Is there a contact at TI for the CIC material ?
Chris Hunt
NPL
>>Reply to your message of 26/06/98 13:15
>Robert,
>
>Copper Invar Copper (CIC) is a Texas Industries "foil" product for
>multi layer boards that was designed to give the resulting board a low
>CTE (coefficient of thermal expansion). The copper is metallurgically
>roll bonded to both sides of a foil layer of Invar (a nickel iron
>alloy that has very low CTE). Invar also has low thermal conductivity
>(much lower than copper). Arlon (among others (not necessarily an
>endorsement :)) makes a laminate core material using CIC. Resulting
>board CTE using CIC and polyimide are 9-12 ppm-C (compared to 16-18
>ppm-C for standard polyimide GI(J,L,N) boards). Talk to your board
>vendors about processing concerns and cost.
>--
>Karl Sweitzer voice: 716.47.77546
>Eastman Kodak Company pager: 716.25.33681
>800 Lee Road fax: 716.47.77293
>Rochester, NY 14650-3118 mailto:[log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>>End of message
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|