TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 17 Mar 2006 16:00:16 EST
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Joe Fjelstad <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
NC drills are highly versatile and stacking panels provides some economy  and
so it will be hard to displace them.

Punching can be fast (all holes at once) but is one at a time and depending
on approach, hole count and feature size the tooling might be costly and  must
be amortized over a number of panels to pay for the tool.

Hole quality is not as good making plating more of a challenge if you plan
on doing double sided PCBs. I have not heard of MLBs being punched  (except
when the drills got too dull ;-)

There should also be some concerned about punching small holes on fine  pitch
in glass fabric as there would be a higher risk of CAF, however  for polymer
films it is not so much of an issue.

I expect there will be other comments coming.

Joe

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2