TECHNET Archives

December 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Date:
Fri, 13 Dec 2013 16:04:57 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Reid <[log in to unmask]>
Message-ID:
Subject:
From:
Paul Reid <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (106 lines)
Hi Wayne,

I agree with your wager. I think that they will fail CAF testing.

The fabricator does not want to pursue CAF testing as it might confuse
the argument.

Sincerely,  

 

Paul Reid 

Program Coordinator  

PWB Interconnect Solutions Inc. 
235 Stafford Rd., West, Unit 103 
Nepean, Ontario Canada, K2H 9C1 

613 596 4244 ext. 229  

Skype paul_reid_pwb 
[log in to unmask] 

 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: December 13, 2013 2:17 PM
To: [log in to unmask]
Subject: Re: [TN] Crazing - the pictures

By the way, I'll wager that 85/85/85 testing with voltage bias will fail
these units.  (for the unfamiliar, that's 85C 85%RH, 85hrs).  Applying
the bias may be a bit problematic with unpopulated boards, but I'm sure
you can come up with something reasonable.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Reid
Sent: Friday, December 13, 2013 12:49 PM
To: [log in to unmask]
Subject: [TN] Crazing - the pictures

Hi Everyone,

 

I finally found Steve Gregory's email address. He has kindly posted some
the pictures of the crazing that I found.

 

http://stevezeva.homestead.com/6494_2_1_mod.jpg

 

http://stevezeva.homestead.com/6494_M_001.jpg

 

http://stevezeva.homestead.com/6496_2_10.jpg

 

 

Sincerely, 

 

Paul Reid 

Program Coordinator 

PWB Interconnect Solutions Inc. 
235 Stafford Rd., West, Unit 103
Nepean, Ontario Canada, K2H 9C1 

613 596 4244 ext. 229  

Skype paul_reid_pwb
[log in to unmask] 

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2