TECHNET Archives

June 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Bloomquist, Ken" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bloomquist, Ken
Date:
Wed, 22 Jun 2005 07:10:27 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (24 lines)
Thank you all for the valuable input as usual. Just to follow up on my
measling problem, we tracked down the culprit. It turns out that our CM
was using too much pressure to swage in the standoffs.

If you remember these are cone swaged standoffs and supposed to be
finger loose but still hold the part perpendicular. They were using just
a little too much pressure and stressing the glass.

Now that they've backed down the pressure the measling has gone away.

Thanks again for all your comments.

KennyB

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2