96 X 10 mil sounds like my kind of pads!!!
I like those dimensions.
Actually it depends on the dimensional tolerance, minimum and maximum
outer dimensions.
I would use 12 mil wide, and 70 to 76 mil long should be sufficient.
I recommend 76 X 12 pads, ( check your component leads will fit at
maximum outer dimension ), solder resist 82 X 18 and solder stencil 76
X 10.
There will be no problems using 96 mil long, it will only improve the
repeatability. If you can get it, use it!!
Regards
Edward Brunker
PSION Computers PLC
ps If you need a skilled Engineer to work in sunny Brazil???????
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|