The problem is the sizing of our current fiducials. They are circles & our board vendor has trouble
producing round level pads on a consistent basis. I believe it is related to their size. Therefore, I
want to make sure that what we are asking for is appropriate.
Golfer wrote:
> Darrell,
>
> Can you inform me of the nature of your problem? What are you trying to
> achieve?
>
> Regards, Graham Naisbitt
>
> [log in to unmask]
>
> Concoat Limited
> Alasan House, Albany Park Phone +44 (0) 1276 691100
> CAMBERLEY GU15 2PL UK Fax +44 (0) 1276 691227
> -----Original Message-----
> From: Darrell Bonzo <[log in to unmask]>
> To: [log in to unmask] <[log in to unmask]>
> Date: 21 October 1998 14:38
> Subject: [TN] Conformal Coating Manufactures
>
> >Is anyone having good success with conformal coating materials other than
> >HumiSeal. I am currently experimenting with different characteristics of
> >these materials, and would appreciate any information concerning different
> >manufactures.
> >
> >Thank You
> >
> >################################################################
> >TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> >################################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in the body:
> >To subscribe: SUBSCRIBE TechNet <your full name>
> >To unsubscribe: SIGNOFF TechNet
> >################################################################
> >Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> for additional information.
> >For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> >################################################################
> >
> >
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
|
|
|