Hi Bev,
Yes exactly -that is what I want to do. Regards Steve
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: February-05-13 8:02 PM
To: 'TechNet E-Mail Forum'; Steven Kelly
Subject: RE: [TN] Nickel sulfamate
Steve,
I will be picky, do you mean plate nickel on to the copper on a PWB FROM a nickel sulfamate solution?
Bev
Blackberry
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steven Kelly
Sent: Tuesday, February 05, 2013 7:44 PM
To: [log in to unmask]
Subject: [TN] Nickel sulfamate
Hi All,
Anyone have any recommendations for someone who can plate nickel sulfamate on a PWB. Thanks. Steve Kelly
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|