TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 5 Sep 2006 09:50:37 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (31 lines)
In a message dated 9/5/06 0:45:08, [log in to unmask] writes:
> Is there a standard that defines a minimum pull force requirement after the
> component has been soldered. 
> A: No, there is no such standard. A properly wetted solder joint is stronger 
than the attachment of the soldering pads to the PCB/component resin matrix.

> The issue is, to get a better joint we had introduced extra solder to the 
> component (confirms to IPC-610D). 
> A: Why do you think that more solder will give you a "better joint"? What 
does better mean?

> Do we have a minimum pull force value which can be adopted so
> that we can give assurance to customer that there will be no issue with
> joints.
> A: Solder joint issues come from either low quality—meaning inadequate 
metalurgical bond due to insufficient wetting; or from creep-fatigue which is not 
very dependent on solder joint volume. So, you are reallly asking the wrong 
question.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2