Raul cantero,
You are asking for a lot of trouble here. What likely would happen with wavesoldering sockets with programmed parts installed is that solder wicks up thru socket pins and solder programmed part pins to socket pins. It would be a big rework hassle to separate the part from the skt.
wavesolder skts and install programmed parts later.
regards
Matthew
Norsat International Inc.
>>> Raul Cantero <[log in to unmask]> January 7, 1999 2:46 pm >>>
Does anyone have any experience inserting programmed parts in sockets PRIOR
to wave soldering the socket into the PWA????
Raśl Cantero
Business e-mail: [log in to unmask]
Personal e-mail: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|