To plate Aluminium you first need to deoxidise it and simultaneously protect
it from re-oxidation which it does immediately in air. This is done using an
alkaline immersion zinc process. Then you [immersion] plate that with nickel
and then you can put your gold on. It's a standard process but from people
who specialise in it. Done properly it can be quite robust (viz Voyager
spacecraft)
--
Regards
Mike
BSP
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Hillman
Sent: Saturday, January 16, 2016 3:42 PM
To: [log in to unmask]
Subject: Re: [TN] plating gold to aluminum
Hi TechNet - another potential issue to consider would be corrosion issues.
Gold is one end of the galvanic table and aluminum is on the other end -
not exactly a metallic pairing I would jump up and down about. The users
should look at the product use environment and assess the potential
corrosion issues.
Dave Hillman
[log in to unmask]
Rockwell Collins
On Fri, Jan 15, 2016 at 5:29 PM, Giamis, Andy <[log in to unmask]>
wrote:
> Au directly to Al?
> I would be concerned over purple plague. Certainly an old problem with Au
> wire bonds on Al chip circuitry.
>
> Ni on Al and Au on Ni are both fairly common. Lots of shops can do that.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Louis Hart
> Sent: Friday, January 15, 2016 5:21 PM
> To: [log in to unmask]
> Subject: [TN] plating gold to aluminum
>
> TechNetters, who in the US knows of a machine shop which can plate gold to
> aluminum? I'm asking on behalf of colleagues and neglected to find out for
> sure if they meant electroplating or some other process. Any ideas would
> be welcome. Louis Hart
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|