Many years ago when the world was less informed than now, I was having
trouble getting people to understand "solderability" and its relationship to
plating.
So I had some paper tissues coated with Sn/Pb. They looked just like un
etched but plated circuit boards.
So I continued to rabbit on about wetting, spread and so on and how just
because you can plate something doesn't mean you can solder it.
Generally to the majority audience's continuing incomprehension, but
then.... It all made sense when I asked a volunteer from the audience to
touch this test substrate with a hot soldering iron. On turning the now
holed substrate over in explanation, someone would invariably shout 451! and
I knew the message had got home.
:)
Regards
Mike
ü Please consider the environment before printing this e-mail
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Saturday, January 15, 2011 2:34 PM
To: [log in to unmask]
Subject: Re: [TN] NTC Friday Element Quiz - the Answer
Denny,
They can plate plastic buttons. That doesn't make plastic a metal.
Bev
----- Original Message -----
From: Dennis Fritz [mailto:[log in to unmask]]
Sent: Saturday, January 15, 2011 09:08 AM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] NTC Friday Element Quiz - the Answer
Hmm, bad choice. Who do I want mad at me - Hillman or Christian? How
about this, from a hip-boot wearing plating guy - if you can electroplate it
(passes current) - does that make it a metal? Electroplated solder or
nickel gold bumps on silicon have been standard practice for decades. I
know, I know, you will tell me silicon is a semiconductor. I guess that
makes it a half-metal for me. Now, either none or both are mad at me.
Denny Fritz
-----Original Message-----
From: Bev Christian <[log in to unmask]>
To: TechNet <[log in to unmask]>
Sent: Sat, Jan 15, 2011 7:07 am
Subject: Re: [TN] NTC Friday Element Quiz - the Answer
Dear Mr. Hillman,
was a little taken aback when in an earlier quiz you labeled antimony as a
etal rather than as a metalloid, but I can live with it, I guess. However,
or you to call silicon a metal is just too much! In 57 years, 41 of those
s a chemist (I am counting from when I decided to be one in grade 9), I
ave NEVER before now heard anyone call silicon a metal. As a main group
hemist (fluorine chemist actually), I consider it a non-metal and am
illing to concede it is a metalloid, but metal? Never! You are poaching,
ir. I will stop short of demanding satisfaction. However, I do ask you to
espond and I also ask fellow TechNetters their opinion on this.
Bev
IM
PS For those of you new to TechNet Dave IS a dear friend and this is all
retty well tongue in cheek. And seeing this venue is overrun with
ngineers, rather than scientists, I highly expect I am going to be
ut-voted, shot down in flames, made into toast and other alliterations.
-----Original Message-----
rom: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
ent: Friday, January 14, 2011 4:03 PM
o: [log in to unmask]
ubject: [TN] NTC Friday Element Quiz - the Answer
Hi folks - Here is the Friday Element Quiz Answer:
The Question:
The first "pure" use of this element began in 1823. This element is
ometimes classified as a metalloid. The density of this element increases
when it is melted. The native oxide of this element prevents further
xidation of the element below 900C. What element is being described?
The Answer:
he element is Silicon (Si). Silicon is a metal that enables technology in
multitude of ways. Silicon is a deoxidizer in steel production, the
asis for integrated circuits, glass, cement, protective coatings for high
emperature applications, and families of polymers. Ge atoms are larger
han Si atoms so an alloy of 85%Si and 15% Ge has an average interatomic
pacing slightly larger than pure Si. When a pure layer of Si is deposited
n the 85/15 alloy, the Si becomes strained resulting in a 70% faster
ignal speed parallel to the surface! Less than 1% of the world's
roduction of Si is the pure form but that 1% (approximately 40K
ons/year) is roughly equal in total dollar value to the other 99% of the
etallic Si production.
Lots of good guesses (this was one of the tougher quizzes) - the winner of
his week's quiz is Bev Christian of RIM. Clumpy have to sneak onto the
380 in Germany and head for Canada:
So far Clumpy has:
Week 1 Lamar Young, SCS Coatings
accomplished nothing (drank lots of coffee)
Week 2 Bev Christian, RIM
conducted REACH material testing
Week 3 Drew Meyer, Benchmark Electronics Inc.
Solderability testing and mowed the lawn
Week 4 Ian Fox, Goodrich
had an epic journey of travel
Week 4 Gary Ferrari, Garrick Global
unknown
Week 5 Fredrick Miller, Astrolab
unknown
Week 6 David Nelson, Raytheon
Was a tackling dummy for Dallas Cowboys
Week 7 Graham Collins, L3 Communications
Cleaned gutters and painted window trim
Week 8 Bill Noel, ITT Geospatial Systems Division
unknown
Week 9 Steve Gregory of RD Circuits
unknown
Week 10 David Bealer of Watchfire Signs
descaled the in-line wash machine! Ouch!
Week 11 Dick Krug of Sparton Corporation
assisted with AS9100 quality management systems requirements audit
Week 12 Steve Creswick of Balanced Enterprise Solutions
Acted as Steve's "go fer" due to a broken leg!
Week 13 Gebhard Neifer, Delphi
conducted a plasma pre treatment Taguchi DOE for a sealing process
Week 14 Bev Christian, RIM
????
Have a good weekend.
Dave Hillman
ockwell Collins
[log in to unmask]
______________________________________________________________________
his email has been scanned by the MessageLabs Email Security System.
or more information please contact helpdesk at x2960 or [log in to unmask]
_____________________________________________________________________
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site
ttp://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
nformation, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
xt.2815
----------------------------------------------------
_____________________________________________________________________
his email has been scanned by the MessageLabs Email Security System.
or more information please contact helpdesk at x2960 or [log in to unmask]
_____________________________________________________________________
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums
or additional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|