What's the PH of the solution?
-----Original Message-----
From: Dhawan, Ashok [mailto:[log in to unmask]]
Sent: Wednesday, December 17, 2003 4:12 PM
To: [log in to unmask]
Subject: [TN] Tarnished Surface
Technetters
Anyone who has experienced and resolved tarnishing of Aluminium surface upon
cleaning with DI water + saponifier. The aluminium surface is protected with
conversion coating (clear) which is turning black when exposed to saponifier
solution.
Ashok Dhawan P.Eng
Manufacturing Engineer
Solectron
Snailmail:1455 Mountain Avenue
Winnipeg MB R2X 2Y9 CANADA
* E-mail: [log in to unmask]
* Phone: (204) 631-7208
* Fax: (204) 631-7294
* I-net: <http://www.solectron.com>
Confidentiality Notice: This e-mail message, including any
attachments, is for the sole use of the intended recipient(s) and may
contain confidential and privileged information. Any unauthorized; review,
use, disclosure or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail and destroy all copies
of the original message.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|