I agree. I would have preferred the spray method. Customer unfortunately is asking for the dip method. Coating will be Acrylic.
Andrew Kettlewell
Sr Process Engineer
Sypris Electronics
Tampa, Fl
-----Original Message-----
From: Bremer, Gary <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, 10 Jan 2006 13:57:53 -0800
Subject: RE: [TN] Manual conformal coat dipping process
Andrew,
Going from spray to dip process you are going to have ripples and drips
that may cause inspection to question the process. There is more
training for the conformal coat operator needed (look for and correct
drips, etc.) prior to being sent to inspection. Your conformal coat
waste is going to be greater.
What type of conformal coat material are you using for this?
Do you already use a spray booth for conformal coating?
Gary Bremer
Senior Manufacturing Engineer
Curtiss-Wright Controls Inc.
Embedded Computing -Subsystem
28965 Avenue Penn
Santa Clarita, CA 91355-4185
Main: 661.257.4430 extension 2170
Fax: 661.257.4782
e-mail: [log in to unmask]
Web: www.cwcembedded.com
NOTICE: This e-mail communication is private and confidential and is
intended for the addressee only. The email may only be used for
conducting business with VISTA Controls Inc., dba Curtiss-Wright
Controls Embedded Computing Subsystems. If you are not the intended
recipient, please notify us by replying to this email followed by
deleting the email and all attachments from your system. Anyone other
than the intended recipient or those with a need to know within the
recipient's organization is strictly prohibited from using, printing,
distributing or disseminating the email or any information or attachment
contained therein.
-----Original Message-----
From: Joseph H. Smith [mailto:[log in to unmask]]
Sent: Tuesday, January 10, 2006 1:41 PM
To: [log in to unmask]
Subject: [TN] Manual conformal coat dipping process
Fellow technetters.
Anyone out there have experience with 'manually' dip coating conformal
coat. I have never done the dipping coating process. Machine spray and
hand spray I have done. The concept sounds simple enough but I was
looking for advice on process got ya's or issues to watch for when doing
the dipping. Our customer is requiring the dipping process and
currently doesn't wish to spend the money on more automated equipment.
Andrew Kettlewell
Sr Process Engineer
Sypris Electronics
Tampa, Fl
___________________________________________________
Try the New Netscape Mail Today!
Virtually Spam-Free | More Storage | Import Your Contact List
http://mail.netscape.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
___________________________________________________
Try the New Netscape Mail Today!
Virtually Spam-Free | More Storage | Import Your Contact List
http://mail.netscape.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|