Hmmmm,
how many pieces an how much may it cost? Idea for higher volume
"mass" production...
- slots plated!!! and tight fit (best capillary effect)
- solder mask around the slots
- boards should get good HAL (is leadfree required - if not, use SnPb
HAL), at least a perfectly wettable surface
- flux abundantly
- good preheating and then dip in a solder bath oder pull it through
the wave.
Could work....
Regards
Matthias Mansfeld
--
Matthias Mansfeld Elektronik * Leiterplattenlayout
Neithardtstr. 3, 85540 Haar; Tel.: 089/4620 093-7, Fax: -8
Internet: http://www.mansfeld-elektronik.de
GPG http://www.mansfeld-elektronik.de/gnupgkey/mansfeld.asc
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------