TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 24 May 2005 14:44:03 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Content-Transfer-Encoding:
7bit
From:
Al Onderick <[log in to unmask]>
Parts/Attachments:
text/plain (59 lines)
Dear Technetters,

            I now have a couple of cross sections to go along with my
xrays.



Does anyone have an idea what might cause this type of anomaly?




http://www.texas-gold.org/PCB/pages/xray/index.htm



Is this a problem or just a strange looking void ?



The board supplier is going to run the following tests



*                    Cross section the 15 pin connector area for optical
microscopy and analysis.

*                    Scanning Electron Microscopy (SEM) analysis of solder
filled and bare silver hole wall surfaces

o                  SEM will identify particulate or other 3-dimensional
bodies to be analyzed with EDS.

*                    Energy Dispersive Spectometry (EDS) analysis of
solder filled and bare silver hole wall surfaces

o                  EDS will identify the all elements relative to the
point of failure to identify possible contributors as the root cause.

*                    X-Ray Fluorescence of bare silver hole wall surfaces

o                  XRF will determine the thickness of the solder deposit
in the hole walls in the 15 pin connector area.



-Al


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2