TECHNET Archives

March 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Tue, 31 Mar 1998 08:18:21 -0500
Reply-To:
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Don Fumia <[log in to unmask]>
Content-transfer-encoding:
7BIT
MIME-Version:
1.0
Organization:
Schneider Automation
Comments:
Authenticated sender is <dfumia@pobox>
Parts/Attachments:
text/plain (44 lines)
Hello TechNet'ers

Palladium.  We recently had a problem with some
SMT capacitors and SMTmetal oxide transient
surpressors which had palladium leads.  The problem
at reflow was tombstoning and mis-alignments.  The
solder appeared grainy and not wetting nicely.   At the
board level other SMT devices appeared acceptible.

I called the manufacturer-no names unless you ask
me off line.  I was informed that we had somehow called
out the incorrect suffix and were receiving palladium coat
on the leads and not tinned leads.  What do we do?

It was recommended by several component manufacturers
that we use a  2% silver content.  Being a little skeptical of
changing our finely tuned process we called all the solder paste
manufacturers.  We were unconditionally guaranteed that
"no problems" would occur with a 2% silver recipe.  We
tried it and it is working great.   My manufacturing engineers
are happy and that makes me happy.  I don't have to look for
alternate sources.

Good Luck.
%&&&&&&&&&&&&&&&&&&&&&&&&&&&%
      Don F. Fumia
      [log in to unmask]
   Schneider Automation
      No. Andover MA
   978-975-9344   FAX x9714
%&&&&&&&&&&&&&&&&&&&&&&&&&&&%

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2