TECHNET Archives

December 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset=ISO-8859-1
Sender:
Subject:
From:
Sasha Miladinovic <[log in to unmask]>
Date:
Tue, 3 Dec 2002 06:29:43 -0600
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Sasha Miladinovic <[log in to unmask]>
Parts/Attachments:
text/plain (35 lines)
Hello Technetters,

I certainly hope that there are people that had faced the same problem as I
am standing in front of right now.
I managed (after a lot of discussions) to convince design department to
start developing PCBs that are exclusively SMD mounted. No problems there
until they needed modular jack that has 6 to 10 circuits and is fully
shielded.
Ofcourse they discovered an alternative that is impossible to reflow.
(Stewart - http://www.stewartconnector.com/drawings/CT750017.pdf ).
Oki.. Not a designer fault this time. Stewart has a problem with this
specific product and the circuit contacts are .14 millimeters above pad
surface and there is no chance we can get a good solder joint there.
Experimenting with a thicker stencil is not an option.
Our distributor talked to Stewart and they said that they are aware of the
problem but are not going to do anything about it now.
I would like to replace Stewart connector with something that is possible
to reflow. Have been looking at Molex, FCI and Kycon alternatives but the
problem there is that they don’t have connectors with 10 circuits. I need a
connector series that has 6 –10 circuits and is equivalent or better than
Stewart alternative.
Volume is 30-40K/Year.
Thnx…

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2