See inset notes below.
-----Original Message-----
<snip>
1. What is the "glass transition" ? What is the glass transitioning from and
to? I'm guessing it's the plastic stage that occurs in a material just
before it melts.
> Glass transition refers to the point where the *epoxy* goes from a
glass-like state
> to a highly plastic state. There are drastic changes to the
materials mechanical
> properties at this point and some can cause PCB failures.
2. What is gained by a higher Tg in tetrafunctional and multifunctional
epoxy-glass?
> Higher Tg materials are needed for applications where thermal
excursion (rapid > temperature changes or wide opperating
temperature range)occur
3. What is meant by the prefixes "tetra" and "multi" as they're applied
here? Is it a reference to the number on bonds in the chemical structure of
the epoxy or glass?
> Di-, Tetra-, and poly- or multi-functional are references to the
bonding structure
> of the epoxy.
<snip>
Jeffrey A. McGlaughlin, C.I.D.
Sr. PCB Designer
Battelle Memorial Institute
Columbus Ohio
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|