TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
John Waite <[log in to unmask]>
Date:
Fri, 22 May 1998 08:25:01 +0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Arnold C. Escanilla" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=ISO-8859-1
From:
"Arnold C. Escanilla" <[log in to unmask]>
Parts/Attachments:
text/plain (87 lines)
Hi John,

Thanks for the advise.
There have been a lot of suggestions about conditioning the photo tool for
24hrs after taking them out of the bag.  We usually only condition them for
4 hours but I'll try your suggestions.  Thanks!
By the way, the dimensional instability problem only happens with our
contacted films and not our plotted ones, but thanks for the input anyway.

Marco



----------
> From: John Waite <[log in to unmask]>
> To: [log in to unmask]
> Subject: Re: [TN] Photo tool stability
> Date: Friday, May 22, 1998 7:46 AM
>
> Just a couple of quick Ideas without diving too deep into  the situation.
>     1) Do you stabilize the film (open the package and "fan" it) for 24
hrs before using in
> plotting.  This should be done in the plotter area
>     2) Are your humidity and temp in the plotting room and other areas
consistent with each
> other?
>     3) Some material movement from the processor is normal (1-2 mils over
the sheet of film).  If
> your shrinkage is constant, size at the plotting/cam station according.
>      There are a number of other items that will also cause this, but
start simple... JOHN WAITE
>
> Marco Biagtan wrote:
>
> > Hi Guys,
> >
> > I have a problem with dimensional stability of photo tools.  The photo
> > tools shrink after processing.  I've tried increasing the drying
> > temperature (50-55C) just so it will not shrink but it still does.
This is
> > really giving me a headache.  Any suggestions?
> >
> > Marco Biagtan
> > NEC-CPI Process Engineer.
> >
> > ################################################################
> > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> > ################################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> > To subscribe:   SUBSCRIBE TechNet <your full name>
> > To unsubscribe:   SIGNOFF TechNet
> > ################################################################
> > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
> > For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> > ################################################################
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2