Can someone explain the reactions of the discoloration for polyimide and
soldermask? These materials would continue to cure with exposure to
extended heat cycles, what is the mechanism of the discoloration? The
materials continue to cross-link, which in the case of soldermask leads to
brittle mask, but what other reactions are taking place and why the color
change?
This just seems like a good day for a chemistry lesson!
Thanks,
Jana Carraway
MSEI
PS - Hans Hinner, how does getting married make your a spud? I come from
Idaho, the potato state, and hence am a "spud"...regardless of marital
state!
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|