Hi there

I urgently need a small quantity of 3M Fluorad FC-725 conformal coat
material.  The earliest shipment 3M can provide is at the end of July.

If anyone could give/sell/loan me a quantity I would be extremely grateful,
and would happily replace once we receive a shipment.  

The product is to be used at a US supplier, and so UK or US sources would be
best.

Thanks in advance



John Loveluck
Group Quality Manager
Tadpole Technology plc
Cambridge Science Park
Cambridge CB4 4RB
Tel: (+44)1223.428200
Fax: (+44)1223.428201

email: [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2