TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dwight Mattix <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Dwight Mattix <[log in to unmask]>
Date:
Tue, 18 Oct 2005 07:19:13 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (121 lines)
At 0.5mm pitch we've had BGA voids large enough to cause adjacent balls to
bridge.  In those cases, it was usually the result of a uVia plating defect
(uVia in the pad).  Makes for an interesting cross-section.

dw


At 06:30 AM 10/18/2005, you wrote:
>         Flux contains acids that when fully activated turn into inert
>chemicals.  It is the acids that when  not fully activated that corrode,
>so acids will corrode metals whether they are trapped or not.  Salts
>with moisture and voltage  make dendrites. They do need free areas to
>grow. In other words salts and resins or rosins will not cause any
>trouble when they are trapped. For the most part with a good reflow
>profile that activates all the acids of the flux will cause no harm if
>trapped in a solder joint. My two non chemistry cents
>         Ramon
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard
>Sent: Tuesday, October 18, 2005 9:02 AM
>To: [log in to unmask]
>Subject: Re: [TN] Voids in BGAs, again
>
>Technet,
>Just wanted to say, yes, very few failures have occurred due to voiding,
>and the situations I pointed out were extreme situations. But the
>interposer attachment failures I described have also happened to others
>in not very severe conditions. There is something about interposer
>attached parts and voids that do not mix well.
>
>Ioan, I may be mistaken, but I was told that flux entrapped inside of
>voids is nothing to worry about because corrosion cannot occur due to a
>lack of oxygen. The voids are sealed. Any chemical or metallurgical
>engineers out there care to respond to this? I would like to know if
>that is true.
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
>Sent: Tuesday, October 18, 2005 7:32 AM
>To: [log in to unmask]
>Subject: Re: [TN] Voids in BGAs, again
>
>Concur with Richard,
>
>good document, professional and academic. But if I am not mistakening,
>it does not mention real failures from voiding.
>
>BTW, your experience is very well appreciated, extreme conditions, bad
>voids. I am wondering if regular testing, like HALT and the others
>caused joints to fail due to voiding.
>
>What about failures due to chemistries, WS flux entrapped into voids
>that corrode their way out?
>
>Best regards,
>Ioan
>
> > -----Original Message-----
> > From: TechNet [SMTP:[log in to unmask]] On Behalf Of Stadem, Richard
> > Sent: Tuesday, October 18, 2005 8:14 AM
> > To:   [log in to unmask]
> > Subject:      Re: [TN] Voids in BGAs, again
> >
> > Thank you Steve!
> > This is an excellent and informational document. Thank you for posting
>
> > it.
> >
> >
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>archives of previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>archives of previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2