Hi Bryan,
I concur with Phil. The holes need to be drilled to spec to begin with,
and have good plating. Amp/Tyco says in their documentation that you
should be able to repair their "Action Pin" compliant press fit
connections once. That means the initial insertion and a repair, and
that's the guideline I always went by. Like Phil, most of the repairs I
did was because of initial insertion problems, one pin folded under, or
a connector off by a row when multiple connectors were pressed in next
to each other.
It's been a little while since I've repaired a connector, but it's just
like Phil says, taking the body apart and pulling it out pin by
pin...fun stuff.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Bavaro
Sent: Wednesday, October 23, 2013 7:44 AM
To: [log in to unmask]
Subject: Re: [TN] Press Fit Connector replacement
I had some experience.....but I have not performed this for about ten
years......
I used to remove and replace press fit connectors when we would have
problems with proper insertion.
It required completely destroying the connector body with cutters and
extracting the compliant pin by pin out of the PWB with a pair of
pliers.
I do not remember damage to the barrel after removal.
The key was having the right amount of copper plating in the barrels.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kerr, Bryan (UK)
Sent: Wednesday, October 23, 2013 6:29 AM
To: [log in to unmask]
Subject: [TN] Press Fit Connector replacement
Hi All
Any views or experience of replacing press fit connectors ? I have some
concerns since I would assume there would be some copper thp distortion
during the first fit and this may affect the reliability of the refit ?
Some internet trawling seems to show that the "compliant" design pins,
where there is a slot in the centre, are more compatible with remove and
replace since some of the distortion will be in the pin. It is a
"compliant" type of pin in my case but could do with some assurance that
this would be OK to do.
Any thought / experiences appreciated
Regards
Bryan Kerr
BAE Systems
********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
________________________________
This message and any attachments are solely for the use of the
addressee and may contain L-3 proprietary information that may also be
defined as USG export controlled technical data. If you are not the
intended recipient, any disclosure, use or distribution of its content
is prohibited. Please notify the sender by reply e-mail and immediately
delete this message and any attachments.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|