Absolutely
Thank you sir.
Barry.
-----Original Message-----
From: d. terstegge [mailto:[log in to unmask]]
Sent: Wednesday, December 17, 2003 1:13 AM
To: [log in to unmask]
Subject: Re: [TN] Rejection criteria for voids in BGA solder joints
Hi Barry,
You forgot to mention the VERY IMPORTANT sentences just above these so
called "requirements":
"The following guidelines are provided as assesment criteria for the
attachment technology process. Without substantial documented
reliability data at the time of publication of this revision, no
acceptability criteria are provided".
Voids larger than 25% which occur as a result of a boarddesign with
via's in pads can be perfectly acceptable and may be just as reliable as
joints without voids !!
Daan Terstegge
Unclassified mail
Personal Website: http://www.smtinfo.net
>>> [log in to unmask] 12/16/03 06:21pm >>>
Ken,
IPC-A-610C Page 12-75 calls out:
Acceptable Class 1,2,3- Less than 10% voiding in the Ball to Board
Interface.
Process Indicator Class 2,3- 10-25% voiding in the Ball to Board
Interface.
-voiding in the BGA solder ball to board interconnection up to 25%may
or may
not be a reliability issue and should be determined in your process
development.
-BGA solder joint reliability studies performed at some industry
locations
show that limited voiding in BGA balls does not impact long term
reliability.
Defect Class 1,2,3- More than 25% voiding in the Ball to board
interface.
Barry
-----Original Message-----
From: Ken Patel [ mailto:[log in to unmask] <mailto:[log in to unmask]>
]
Sent: Tuesday, December 16, 2003 10:09 AM
To: [log in to unmask]
Subject: [TN] Rejection criteria for voids in BGA solder joints
All,
What are the current rejection criteria for voids in BGA solder joints?
I am
preparing assembly notes in this regards.
Any help will be highly appreciated.
Re,
Ken Patel
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
<http://listserv.ipc.org/archives>
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|