TECHNET Archives

December 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 27 Dec 2004 16:33:00 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ertugrul Cakir <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
Ertugrul Cakir <[log in to unmask]>
Parts/Attachments:
text/plain (25 lines)
There is a different information in IPC 610 and IPC6221 about clinch
angle. According to IPC 610, lead terminations are clinched a min. 45
degree and the target is 90degree (page 93). And according to IPC 6221;
clinched leads are bent between 15 and 45 degree as measured from a
vertical line perpendicular to board (page 64). If we think automatic
insertion (axial and radial insertion) especially in assembly production
what should be the acceptance clinch angle area.

best regards,






---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2