TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Brian Ellis <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Thu, 1 Jul 2010 10:28:33 +0300
Content-Type:
text/plain
Parts/Attachments:
text/plain (72 lines)
Did Marc Bituagan deliberately do exactly what I urged him not to, to
cock a snook at my plea?

Brian

Brian Ellis wrote:
> I'm sorry, but a few members here seem to have ignored, of late,
> reasonable discipline in the use of threads.
>
> Background: many members use their e-mail clients to sort the posts into
> threads. This has the advantage that, theoretically, the initial post is
> followed by all the answers in chronological and hierarchical orders.
> This makes following a subject easy-peasy-lemon-squeezy. The other
> choices are purely chronological, which means that related posts may be
> separated by a dozen others on half-a-dozen different subjects.
> Alternatively, users may manually sort their messages.
>
> Problem: some members, who may be unaware of the advantages of threading
> in their e-mail client, start a new and unrelated subject by clicking
> 'Reply' in an existing thread. This new subject therefore appears to be
> a reply to the old subject, when it is nothing of the sort. This can be
> repeated ad infinitum, or rather ad nauseam. One thread recently housed
> six different and unrelated subjects mixed higglety-pigglety.
>
> Solution: I URGE members here to:
> - a) always to start a new subject by addressing the post to Technet
> from their address book; NEVER start a new subject by using 'Reply' or
> 'Reply All'.
> - b) always to reply to an existing subject by clicking 'Reply' or
> 'Reply All'; NEVER start a new thread for an existing subject.
>
> Thank you all for listening to my heartfelt plea!
>
> Brian
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2