Supposedly gold ball bonding can be performed at room temperature with a
high frequency ultrasonic generator. There was just an article in one of
the trade journals (Semiconductor International, August Issue) regarding
room temperature bonding. Haven't tried it yet.
One can make a bond stick at room temperature with a normal ultrasonic
generator, but I would question the reliability of that bond. There would
probably be mechanical forces holding the bond down, but not a true weld.
As for the capillary, I'm not sure that you can get one with those
dimensions. K & S Micro-Swiss (and others I imagine) sell bottleneck
capillaries, but I think their standard bottleneck height is 18 mils with a
tip diameter of 6 mils. This capillary can handle 0.7 - 1.3 mil wire. I
have a 1990 catalog, so maybe there have been improvements since then, but
50 mils would be a stretch I think.
Dave Anderson
>>> <[log in to unmask]> 08/15/97 12:54pm >>>
Hello Everybody,
I had a couple questions concerning gold ball bonding. First I was
wondering
about the feasability of gold ball bonding without using heat. Second,
What
is the finist tip on a capillary that can be made for a deep access
application
The diameter can not be greater than 9.5 mils at 50 mils up from the tip.
If
such a cap is possible to make what diameter wire would be used.
Thanks for the help,