Mel pointed you to the right direction. Last week Doug Pauls was more
specific about it.
Yes, J-STD-001 establishes acceptability requirements that include
requirements for Fluxes (J-STD-004), solder alloys (J-STD-006) and solder
pastes (J-STD-005).
The IPC-HDBK-001 is a good place to get information to properly apply the
standards.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of John Foster
Sent: Thursday, August 18, 2005 11:41 AM
To: [log in to unmask]
Subject: [TN] Class 3
I am not sure if this is the right forum for this question.
We may have a requirement to assemble to class 3.
I have a copy of ipc-a-610 and my impression is that this is more of inspect
to class 3 kind of thing. Does class 3 assembly have requirements for
fluxes, solders etc etc
Any input will be greatly appreciated.
Thank You
John Foster
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|