TECHNET Archives

September 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Peter G. Houwen" <[log in to unmask]>
Date:
Fri, 25 Sep 2015 09:30:24 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (22 lines)
DFR need a lot more.  here is the flavor
http://www.dfrsolutions.com/software/see-what-sherlock-can-do-for-you-2/
> It depends.
>
> There are SO many factors affecting initial joint strength, pad size being
> just one.  The perfect pad size, in the wrong place, with the wrong solder
> or poor processing can make a very weak joint.
>
> And still, it's no measure of reliability.  Poor solder joints are more
> likely to be weak.  Poor solder joints are more likely to be less
> reliable.  But poor older joints could pass an initial pull test and still
> propagate cracks and fail later in life.
>
> Peter
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2