Hi folks! Cupron is a member of the cupronickel family and has all the
joyful solderability issues/constraints of nickel due to the percentage of
nickel contained in the alloy. A cupronnickel alloy is difficult to solder
using traditional electronics soldering practices.
Dave Hillman
Rockwell Collins
[log in to unmask]
Steve Kelly
<[log in to unmask]> To: [log in to unmask]
Sent by: TechNet cc:
<[log in to unmask]> Subject: Re: [TN] Cupron solderability
11/07/2003 11:10
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Steve
Kelly
Is cupron – cupro-nickel? It is very difficult to wet. When we do this we
usually put kapton tape on top of the part to hold it down because the
solder joint is so weak. Regards Steve Kelly
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glenn Pelkey
Sent: Friday, November 07, 2003 11:59 AM
To: [log in to unmask]
Subject: [TN] Cupron solderability
Hi folks,
Anyone familiar with Cupron and if it is solderable?
Checked Matweb, but no indication on solderability. Basically, it is
a copper and nickel alloy, although some show an iron component. A
quick test here with a sample showed no wetting action, even with an
aggressive flux. There is no surface finish to protect the copper or
nickel from oxidation.
Thanks,
Glenn
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
|
|
|