Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0u0cII-00006eC; Sat, 23 Mar 96 17:00 CST |
X-PS-Qualifiers: |
/FONT=Courier-Bold/LINES=66/LEFT_MARGIN=36/CALCULATE/TOP_MARGIN=36/BOTTOM_MARGIN=36 |
X-VMS-To: |
|
Date: |
Sat, 23 Mar 1996 14:58:12 -1000 |
MIME-version: |
1.0 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
From [log in to unmask] Mon Mar 25 12: |
40:36 1996 |
X-Loop: |
|
Old-Return-Path: |
|
Resent-Message-ID: |
<"hta6O.0.Yk8.5A8Ln"@ipc> |
Subject: |
|
Message-id: |
|
Content-transfer-encoding: |
7BIT |
X-VMS-Cc: |
DOUG_M2 |
Organization: |
VeriFone |
From: |
|
Parts/Attachments: |
|
|
I would suggest you do one of two things.
1. retest your boards for solderability as you normally do for incoming
testing. If you don't know how to do this, you should ask your PCB
supplier to help you or go to his place and have him demonstrate it to you
and then you can go back to your factory and implement this into IQC.
2. You can return these boards to your PCB supplier and ask him to reclean
them for oxide removal. He probably already has this process and it is
what he will do on many of his own boards before he send them out to his
customers. As part of the recleaning he should retest them for
solderability for you and supply you with the test board which demostrates
that it is solderable
Doug
From: IN%"[log in to unmask]" 15-MAR-1996 05:40:02.97
To: IN%"[log in to unmask]"
CC:
Subj: ASSY
I have a six layer board (FR4) that has been setting on the shelf for three
years, and not stored in plastic bags.
What would be your recommendation to assure that these boards would solder
properly, when processed?
Thanks In Advance
Michael Cussen
Medar Inc.
mcussen@medar
|
|
|