TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Kelly <[log in to unmask]>
Date:
Tue, 14 Jul 2009 17:55:21 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Syed Ahmad <[log in to unmask]>
Subject:
From:
Syed Ahmad <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<007801ca04b6$e1aa6500$a4ff2f00$@com>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (54 lines)
You need to know activation energy for degradation and then calculate life
at desired temperature.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Kelly
Sent: Tuesday, July 14, 2009 2:11 PM
To: [log in to unmask]
Subject: [TN] Storage life for rigid flex

Good Afternoon,

We have a program for some reasonably simple rigid flex (4-8 layer) where
the requirement is a 20 year life in storage conditions from -40C to +125C.
Is there any evidence that polyimide rigid material and pre-pregs would be
better than a good FR-4 (170C) for long term reliability. Thanks. Steve
Kelly



Steve Kelly (PLEASE NOTE NEW E-MAIL ADDRESS)

(416) 750-8433 (work)

(416) 750-0016 (fax)

(416) 577-8433 (cell)




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2