Hi TechNet! Bill is correct! The phase diagram that Michael found out on
the web is very incorrect! I didn't pay much attention when I first took a
look at it but that diagram is wrong. It shows a eutectic temperature of
175 and eutectic end points of approximately 10% and 91% when they should
be 183C, 19% , and 2.5% respectively. I would suggest we find a better web
reference than this. Jason - did you receive an accurate Pb/Sn phase
diagram? What I faxed over is not correct!
Dave Hillman
Rockwell Collins
[log in to unmask]
Bill Davis <[log in to unmask]> on 05/12/99 10:30:58 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Bill Davis <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: Re: [TN] phase diagram
Not sure about this phase diagram- it shows eutectic at 175. I always
thought that it was 183...
> Bill Davis, Ph.D.
> Diamond Multimedia Systems
> Senior Scientist
> Tel. 408.325.7868
> Cell. 408.888.5650
> e-mail: [log in to unmask]
>
-----Original Message-----
From: Alderete, Michael [mailto:[log in to unmask]]
Sent: Tuesday, May 11, 1999 10:40 AM
To: [log in to unmask]
Subject: Re: [TN] phase diagram
Jason-
See diagram on page
http://www.met.kth.se/pd/element/Pb-Sn.html
-Michael Alderete
jason Smith wrote...
------------------------------
Date: Mon, 10 May 1999 10:43:26 -0400
From: Jason Smith <[log in to unmask]>
Subject: Re: phase diagram
Can anyone email me a eutectic diagram for Pb/Sn? I would appreciate
it.
Jason Smith
Process Materials Engineer
Lexmark Electronics
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|