TECHNET Archives

April 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Hernefjord Ingemar <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Date:
Wed, 9 Apr 2008 08:34:57 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (48 lines)
What corrosion? Internal (the solder joint itself) or external
(surrounding) ?
If the silver was free, I could think of migration, but the silver isn't
free.
Never heard of corrosion caused by silver content in the solder, at
least not for normal applications. 

Inge 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of - bogert
Sent: den 8 april 2008 23:27
To: [log in to unmask]
Subject: [TN] Sn62 solder; any negative experience using it???


April 8, 2008

Sn62 solder contains 2% silver.  Have folks experienced any issues using
SnPb solder with this much silver?  The historical QQ-S-571E solder spec
indicated that using Ag2.5 solder can result in corrosion issues in a
humid environment but I am not aware of any issues using Sn62 solder.
My understanding is that using 2% silver helps when soldering to ceramic
parts having palladium/silver finish.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2