TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Wed, 22 Sep 1999 11:37:25 +1000
MIME-Version:
1.0
X-To:
Les Hughson <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Klasek <[log in to unmask]>
Parts/Attachments:
text/plain (96 lines)
I'd go with silicon Les ;
when in open outdoor elements ; anything else is struggling to meet it's
resilience .
I've have a various profiles, shapes and application prototypes being truly
life tested
anchored in cliff rock in pounding surf for a couple of years on one of my
locations :

everything else (epoxy, metals, urethanes, cements, socalledsuperglues,
etc.)
gave up within months in waves, salt, sand, and UV.
Even crabs don't like it ; human's ain't around (need to absail to it) ;
so silicon lives well in most applications ;
(unless misdesigned by Dow)

Your's is obviously design dependent as well : experiment .

Paul Klasek
ResMed

PS

CLEAR moisture fav is definitely Si.
But you have to have design consideration on application :
For example lip inwards to hold the silicon plug = passive mechanics needed
;
silicon is a sealant , not adhesive .
I'd distrust adhesives in general anyhow (aging)


-----Original Message-----
From: Les Hughson [mailto:[log in to unmask]]
Sent: Wednesday, 22 September 1999 10:42
To: [log in to unmask]
Subject: [TN] Moisture Proof Encapsulation


I have a small temperature sensor pcb which is to be sealed into an
enclosure, one side of which is in contact with warm water and may leak
slightly, the other side is in air, probably encountering condensation.

My problem is how to get impartial advice on what is the best type of
encapsulation compound to use. e.g. Silicone Rubber, Epoxy Resin,
Polyurethane Resin etc. Various manufacturers all have their own range of
products and will recommend one from there range but I have not found a
single source which manufactures the various different types of compound
listed above and can tell me which would be best.

So. Does anyone have any experience of comparing these different types of
materials...

Silicone Rubber.
Epoxy Resin.
Polyurethane resin.
Others?

Is there a clear favourite for moisture protection?

Any advice would be much appreciated. :-)


Les Hughson, BEng.
Product/Software Engineer
Spa-Quip Ltd
Tel (+649) 415 8622
Fax (+649) 415 8621

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2