Chris:
At risk of repeating myself, ionic contamination is almost always a result of
a SLOWLY dissolving metal deposit, likely in your case to be imbedded pumice.
You need a chemical clean that will dissolve that residue. In your case, you
may be lucky, and it may be as simple as a simple acid wash. If that is the
case, it could be rapid, and run unheated.
If however, the laminate/soldermask has reacted with the metallics, you will
need an alkaline, chelated, product, which will take longer, and require a
heated solution.
A number of vendors supply such chemistry, including us.
Contact me directly, if you would like more information, or samples of our
magic.
Rudy Sedlak
RD Chemical Company
[log in to unmask]
phone 650-962-8004
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|