Hello Dick,
It is definitely possible. However, it is extremely important to properly
control plating parameters that effect plating distribution. Also,
depending on how well you control the process, you may have to use
excessive border around the panel to isolate the circuits from your high
current density area (robbers).
Good Luck
At 11:13 AM 7/22/98 EDT, you wrote:
>Technetters
>
> Is it possible to produce 5/5 technology with a panel plate tent and etch
> process ? Also, what are the strengths and weaknesses of horizontal plating
>processes ? Can anyone provide me with info on horizontal electro plating ?
> Thanks for your help
>
>Dick Desrosiers
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|