TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Chellis, Tammy" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Chellis, Tammy
Date:
Fri, 19 Nov 2004 12:33:02 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (25 lines)
We do incoming inspections on the PCB and we are having troubles with
identifying if variations in the LPI layer is acceptable. We are having a
problem with coverage on the Vias. I
have a customer who specifies the vias are plugged and tented. I am getting
boards with a copper color at some of the vias. I have tried to solder and
it
will not take the solder but using a DMM the via is not electrically
isolated. I am not sure if this is a problem or not. Is a board in IPC
compliance
with out electrical isolation of a plugged and tented via?
The tenting is to be done with the LPI layer and appears to be very thin
on some vias. We are not trying to solder to them I just tiring to find out
if it is a defect. The thing that does not make sense to me is the
conductivity to the via.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2