Hi Don,

We're presently doing some plating line antifungal investigation in the lab
at Electrochemicals but not related to the rinse after the acid cleaner.
 We're working down the line....where plating "threads" prevail?  Interesting
that this could come from the acid cleaner.  We'll look into it and advise.

Regards,

Roger Mouton