Steve,
I used their bar solder years ago at a small shop in Silicon
Valley that was very cost (and quality) conscious, and never had a
problem with the raw material or the finished results. Dross generation
was also reduced quite a bit with the electrolytic bar. Customer service
was very good, with a full range of analytical services available for
bath monitoring.
Mike McMonagle
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, August 26, 2003 8:19 AM
To: [log in to unmask]
Subject: [TN] Electrolytic Solder
Mornin' again!
We've been approached recently by a company named Metallic Resources
( http://www.metallicresources.com ) that makes a solder they call
"Four 9's"
( 99.99% pure), and they do it by using a proprietary electrolytic
process.
They make a lot of claims about their solder. I was wondering if anybody
uses their solder, and if everything they say about their solder is
true.
Thanks!
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|