A punched PWB results in frayed edges susceptible to moisture ingress and thus delamination. This is not a standard practice. I believe IPC does not support this process.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Colin McVean
Sent: Wednesday, August 09, 2006 10:44 AM
To: [log in to unmask]
Subject: Re: [TN] Routed edge tolerance
A punched FR4 4 layer? Good grief!
Colin McVean M.Inst.C.T.
Production Manager
Artetch Circuits Limited
Main: 01903 725365
DD: 01903 712926
Email: [log in to unmask]
www.artetch.co.uk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of arnaud grivon
Sent: 09 August 2006 16:28
To: [log in to unmask]
Subject: Re: [TN] Routed edge tolerance
Jim,
I won't be able to answer your question, but just want to share a past
experience with punched PCB.
Punched PCBs have rough edges compared with routed PCBs. These rough
edges make it easier for water to run along the glass fibers of the PCB
and can create short circuits with internal power planes. This was the
root cause of catastrophic failures (burning) occuring on an electronic
equipment (I cannot disclose the details).
Granted, the product was poorly designed as the power plane was close to
the PCB edges (By the way, it was also a price sensitive 4 layer PCB).
Just a thought.
Best regards,
A. Grivon
James Verrette a écrit :
> I am trying to figure out what the minimum clearance would need to be
> between a PCB and a housing that it fits into. The piece I am not sure
> on is the tolerance of the routed edge of the PCB. The PCB is about
> .050 thick and the outline is quite complex with curved edges and
> cutouts. What is the maximum variation in the routed edge that I can
> expect from the typical mid-high volume board fabricator? I have been
> told +/-.005 hole to edge and +/-.005 edge to edge. But what is the
> yield at this tolerance? It is just for straight line routs? The board
> is 4 layers and cost sensitive, so we don't want to over specify the
> edge dimension tolerance and drive up cost or limit ourselves to select
> few board shops.
>
> I have also seen quotes from Asian sources recommend punching instead of
> routing. Where is a good source of layout design guidelines for this
> process? Does it yield good results? I have some knowledge of
> singualtion punching, but not in the board fabrication process.
>
> Jim Verrette
> Electrical Engineer
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|